Hastelloy C Chemical composition
Alloy | % | Ni | Cr | Mo | Fe | W | Co | C | Mn | Si | V | P | S |
Hastelloy C | Min. | bal | 14.5 | 15 | 4 | 3 | |||||||
Max. | 16.5 | 17 | 7 | 4.5 | 2.5 | 0.08 | 1 | 1 | 0.35 | 0.04 | 0.03 |
Hastelloy C Physical properties:
Density | 8.94 g/cm3 |
Melting point | 1350 ℃ |
specific heat capacity | 0.385 103J/kg•K |
coefficient of thermal conductivity | 29.3 W(m•K) |
elastic modulus | 210 103MPa |
Hastelloy C alloy mechanical properties in the room temperature
Alloy Status | Tensile strength | Yield strength RP0.2 N/mm² | Elongation |
Bar | 690 | 315 | 30 |
Hot rolled plate | 690 | 315 | 30 |
Cold rolled plate | 690 | 285 | 40 |
Strip | 690 | 315 | 30 |